DURACAST-XE is a high heat
investment comprising of a large fraction of microfine particles
for smoother mix for investing the mold. DURACAST-XE
minimizes entrapment of air bubbles during mixing which
results in a cleaner casting in all types of alloys - from
noble alloys (gold alloys) to non-precious alloys.
Ringless castings: Use a very slow burnout method
(3 to 5 degrees F per minute).
Molds in a metal casting ring:
Slow or Fast burnout starting at 600 F.
DURACAST-XE offers:
- Long working time
- Ultra smooth flow / easy mix
- HIGH setting and thermal expansion for batch consistency
- Smoothest castings - ABSOLUTELY
- Reduced finishing time
- Less use of finishing materials
- Very little or no rework.
|
|
Physical Properties @
72 F (22 C):
|
|
All tests conducted with
full strength liquid.
|
|
Liquid-to-powder ratio
|
27 / 100
|
|
Working Time (minutes)
|
4-6
|
|
Setting Time (minutes)
|
15 Max
|
|
Expansion:
|
 |
|
Setting
|
2.4 %
|
|
Thermal
|
1.6 %
|
Packaging
|
XE-160
|
36, 60gm + liquid
|
|
XE-190
|
24, 90gm + liquid
|
|
XE-260
|
144, 60gm + liquid
|
|
XE-290
|
100, 90gm + liquid
|
|
XE-360
|
72, 160gm + liquid
|
|
XE-901
|
12, 1kg + liquid
|
|
10151
|
Special Liquid 900 ml
|
|
10161
|
Hi-Expansion Liquid 900 ml
|
|